A question? Visit our contact page

LINCORE® 57-G provides quality resistance and moderate impact resistance when tempered with proper preheat and interpass temperature, exceeds typical application requirements in regeneration, repairs in mining and agricultural segments.

What's Included?

  • (1) 25 lb Plastic Spool

Features

  • Maintain resistance to check cracking with proper preheat and interpass temperature
  • Can be used with the bulk tungsten carbide process for additional abrasion resistance and exceptional wear life
  • Designed to meet the weldability and mechanical property needs of mining equipment suppliers and rebuilders
  • The hard martensitic matrix provides good metal-to-metal wear resistance and moderate impact resistance when tempered
  • Diameter: 1/16 in (1.6 mm)
  • Welding Process: MCAW
  • Approximate Current: 220-415 Amps
  • Voltage: 23-32 Volts
  • Wire Feed Speed: 3.8-11.4 m/min (150-450 ipm)
  • Deposition Rate: 2.4-7.1 kg/hr (5.2-15.7 lb/hr)
  • Consumables Material: Gas Metal-Cored (GMAW-C) Wire
  • Rockwell Hardness: 56-61 Rc
  • Mass Loss: 0.36 g (ASTM G65)
  • Deposit Carbon Content: 0.9-1.1%
  • Deposit Chromium Content: 7.6-10.0%
  • Deposit Niobium Content: 1.3-1.8%
  • Deposit Manganese Content: 1.2-1.6%
  • Deposit Molybdenum Content: 0.5-0.6%
  • Deposit Silicon Content: 0.8-1.2%
  • Deposit Vanadium Content: 1.4-1.9%
  • Winding: RDM
  • Country of Origin: United States
  • Warranty Length: 1 Year

Downloads

    Specsheet