A question? Visit our contact page

Designed to meet the specific requirements of spiral pipe seam welding of up to API X80 grade pipe. High speed welding capability for increased productivity. Capable of producing weld deposits with impact properties exceeding 27 J (20 ft· lbf) @ -51° C (-60° F) with Lincolnweld® LA-81. Smooth bead profile achieves optimal appearance on both inner and outer diameter welds. Self-peeling slag allows for clean and easy slag removal for reliable non-destructive testing results.

Features

  • Actual (Type 3.1) certificates for each lot of flux showingchemical composition, particle size and moisture level areavailable in the certificate center of lincolnelectric.com
  • High speed welding capability for increased productivity
  • Smooth bead profile achieves optimal appearance on both innerand outer diameter welds
  • Designed to meet the specific requirements of spiral pipe seamwelding of up to API X80 grade pipe
  • Self-peeling slag allows for clean and easy slag removal forreliable non-destructive testing results
  • Capable of producing weld deposits with impact propertiesexceeding 27 J (20 ftlbf) at -51°C (-60°F) withLincolnweld® LA-81

What's Included?

  • (1) 2600 lb Bulk Bag
  • Weight: 2600 lb
  • Weld Grade: API X80
  • Impact Energy: 27 J (20 ft lbf) at -51 C (-60 F)
  • Welding Process: SAW
  • Alloy Type: MSLA
  • Consumables Material: Submerged Arc (SAW)
  • LECO Consumable Diameter: Flux
  • Country of Origin: United States