Hot Work (H-10 to H-16) Tool Steel ELECTRODE

  • Electrode Diameter: 3/32 in
  • Material: Hot Work Tool Steel
  • Hardness: 52-56 Rockwell C
  • Preheat Temperature: 800ºF
  • Annealing Temperature: 1500ºF to 1550ºF
  • Hardening in Air Temperature: 1800ºF to 1900ºF
  • Hardening in Oil Temperature: 1750ºF to 1850ºF
  • Welding Current: 50-90 A (3/32 in electrode)
  • Polarity: DC Reverse (DCEP) or AC (DCEP preferred)
  • Alloy Composition: 5% Chromium-Molybdenum-Tungsten
  • Steel Type: Tool Steel H-12