ER385 is a high alloy austenitic stainless steel used to weld base metal of similar composition and with its extra low residual elements such as C, Si, S, P , and N improves the weld metal from hot cracking & fissuring.904L with it 20% Cr, 25% Ni,4.5% Mo and1.5% Cu is often found to manufacture or repair processing equipment, tanks, vessels, and piping that handles acetic & sulfuric acids and other chlorides. Also used for joining 317L & 904L to 304 or 316whereaddedcorrosion resistance is needed. Ar + 30% He +1-3 %CO2recommended

  • Size: 0.035 in
  • Alloy Type: ER904L (ER385)
  • AWS: A5.9 ER385
  • Weight: 33 LB
  • Chromium Content: 20-21.5%
  • Nickel Content: 24-26%
  • Molybdenum Content: 4.2-5.2%
  • Copper Content: 1.2-2.0%
  • Carbon Max: 0.025%
  • Silicon Max: 0.50%
  • Phosphorus Max: 0.020%
  • Sulfur Max: 0.03%
  • Manganese Content: 1.0-2.5%
  • Tensile Strength: 82,200 psi
  • Yield Strength: 55,000 psi
  • Elongation: 35%
  • Gas Mix Recommended: Ar + 30% He + 1-3% CO2