A question? Visit our contact page

ER410 stainless steel welding wire is used to weld straight chromium steels such as AISI types 403, 405, 410, 414 and 416. It is also used as an overlay on carbon steels to give added resistance against corrosion and abrasion. Preheat and post-heat treatment is required.

  • Alloy: ER416
  • Weight: 33 lb
  • Wire Diameter: 1/16 in.
  • Material: Stainless Steel
  • Preheat Temperature: 350-500 F
  • Postheat Temperature: 1350-1400 F
  • Postheat Duration: 1 hour per inch
  • Typical Tensile Strength: 80,000 psi
  • Typical Yield Strength: 44,000 psi
  • Elongation: 26%
  • Typical Chemistry - Carbon: 0.08%
  • Typical Chemistry - Manganese: 0.50%
  • Typical Chemistry - Silicon: 0.40%
  • Typical Chemistry - Molybdenum: 0.15%
  • Typical Chemistry - Sulfur: 0.03%
  • Typical Chemistry - Chromium: 12.90%
  • Typical Chemistry - Nickel: 0.40%
  • Specifications: ANSI/AWS A5.9 ER410, ASME SFA 5.9 ER410

Downloads

    Certificate
    Safety Data Sheet
    Product sheets