Washington Alloy Aluminum Bronze A-3 contains a higher Iron (Fe) content than Aluminum Bronze A-2. The higher Iron content gives “A-3” greater strength when joining aluminum bronze castings of similar composition

  • Tensile Strength: 65,000-110,000 psi
  • Yield Strength: 35,000-48,000 psi
  • Brinell Hardness: 140-185
  • Size: 1/8 in. x 36 in
  • Weight: 10 lb
  • Alloy Type: Aluminum Bronze A3 ERCuAl-A3
  • Iron Content: 2.0-4.5%
  • Aluminum Content: 10.0-11.5%
  • Zinc Content: 0.10%
  • Silicon Content: 0.10%
  • Lead Content: 0.02%
  • Copper Content: Remainder
  • Density: 0.269 lbs/in3
  • Electrical Conductivity: 12% of IACS
  • Thermal Conductivity: 34 Btu
  • Solidus Temperature: 1880 F
  • Liquidus Temperature: 1900 F
  • Compliance: AWS A5.7 ERCuAl-A3 Class F-36