A question? Visit our contact page

Washington Alloy Aluminum Bronze A-3 contains a higher Iron (Fe) content than Aluminum Bronze A-2. The higher Iron content gives “A-3” greater strength when joining aluminum bronze castings of similar composition

  • Alloy Type: Aluminum Bronze A3 ERCuAl-A3
  • Wire Diameter: .045 in
  • Weight: 10 lb
  • Tensile Strength: 65,000-110,000 psi
  • Yield Strength: 35,000-48,000 psi
  • Brinell Hardness: 140-185
  • Elongation: 22%
  • Density: 0.269 lb/in3
  • Thermal Conductivity: 34 Btu
  • Electrical Conductivity: 12.0% IACS
  • Solidus Temperature: 1880 F
  • Liquidus Temperature: 1900 F
  • Iron Content: 2.0-4.5%
  • Zinc Content: 0.10%
  • Silicon Content: 0.10%
  • Aluminum Content: 10.0-11.5%
  • Lead Content: 0.02%
  • Copper Content: Remainder
  • Specification Standard: ANSI/AWS A5.7, ASME SFA 5.7

Downloads

    Tech data sheet