A question? Visit our contact page

Stainless Steel TIG

  • Diameter: 3/32 in
  • Length: 36 in
  • Tensile Strength: 150,000 psi (typical, heat treated)
  • Yield Strength: 135,000 psi (typical, heat treated)
  • Elongation: 10%
  • Welding Current: 60-210 A
  • Arc Voltage: 16-30 V
  • Wire Feed Speed: 100-330 ipm
  • Gas Flow: 20-30 cfh
  • Recommended Gas: 90% Helium, 7.5% Argon, 2.5% CO2 or Argon with 1-5% Oxygen
  • Type: TIG Wire
  • Alloy: 630 (17-4 PH) Stainless Steel
  • Material: Martensitic Stainless Steel
  • Specification Standard: AWS A5.9/A5.9M
  • Post Weld Heat Treatment: Heat to 1875-1925°F, hold 1 hr, air cool; precipitate harden at 1135-1165°F, hold 4 hr, air cool
  • TIG Tungsten: 2% thoriated (Red Band)
  • TIG Gas Flow: 15-30 cfh
  • Recommended Gas Cup Size: 3/8 in to 1/2 in
  • Weight: 10 lb

Downloads

    Safety Data Sheet
    Spec Sheet