Chrome-Nickel-Moly (8620) Tool Steel ELECTRODE

  • Welding Current: 50-90 A (Stick Electrode)
  • Welding Current Polarity: DC Reverse Polarity (DCEP) or AC
  • Preheat Temperature: 300ºF to 400ºF for 8620 steel
  • Tensile Strength: Up to 105,000 psi
  • Hardness: 25-30 Rockwell C as welded
  • Diameter: 3/32 in
  • Material: Chrome-Nickel-Moly Steel (8620)
  • Weight: 5 lb