A question? Visit our contact page

Offers superior puddle control in all positions, virtually effortless slag removal, and excellent bead wetting. It can potentially reduce the level of preheat normally used on crack sensitive steels.

Features

  • Capable of producing weld deposits with tensile strength exceeding 620 MPa (90 ksi)
  • Designed for welding with 75-95% Argon/Balance CO2 shielding gas
  • Use on high strength, low alloy steel applications
  • H8 diffusible hydrogen levels

What's Included?

  • (1) 25 lb Spool
  • Consumable Diameter: 0.045 in (1.1 mm)
  • Tensile Strength: 90 ksi
  • Hydrogen Level: H8
  • Shielding Gas: 75-95% Argon, Balance CO2
  • Spool Weight: 25 lb
  • Consumables Material: Flux-cored (FCAW-G) Wire
  • Winding: RDM
  • Classification: E91T1-M21A0-K2-H8
  • Welding Process: FCAWG
  • Alloy Type: SLA
  • Country of Origin: United States