A question? Visit our contact page

TECHALLOY® 99 produces welds more machinable than a Tech-Rod® 55 and is ideal for the repair of castings deposit, preheat and inter-pass temperature is required on cast iron to minimize the potential for cracks during welding.

Features

  • Q2 Lot® - certificates showing actual wire composition available online
  • Welds produced are generally more machinable than a Tech-Rod® 55 deposit
  • A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks

What's Included?

  • (1) 33 lb Spool
  • Consumable Diameter: 0.045 in (1.1 mm)
  • Alloy Type: HSR
  • Spool Weight: 33 lb
  • Material: MIG (GMAW) Wire
  • Winding: PLW
  • Welding Process: GMAW
  • Classification: AWS ERNi-CI
  • Country of Origin: United States
  • Warranty Length: 1 Year
  • Preheat Temperature: 350 F (175 C)