A question? Visit our contact page

LINCOLN® SHS® 8000W Wire Arc Spray hardness increases as a function of time and temperature for typical application on Boiler Tubes, Oil & Gas Power Generation, Pulp & Paper. This procedure was developed on a TAFA 8830/8835 system. Changes in equipment, materials, and substrates may change optimum procedures. Listed procedures should only be used as a starting point.

Features

  • Superior bond strength without necessity of bond coat
  • Hardness increases as a function of time and temperature
  • Excels in elevated temperature environments where fly ash and bed ash erosion occurs

What's Included?

  • (1) 25 lb PLW Spool
  • Wire Diameter: 1/16 in (1.6 mm)
  • Spool Weight: 25 lb
  • Material: Wire Arc Spray (THSP-ASP)
  • Country of Origin: Multi Country
  • Warranty Length: 1 Year