Designed for single or multipass welding where high strength and impact toughness is required, weld metal tensile strengths of 80 ksi (552 MPa) are maintainable after long term stress relieving (50 hr or more). The presence of nickel in the wire chemistry helps increase low temperature impact toughness 13.2 lb/hr at 400 amp deposition rate, 99% efficiency.

  • Tensile Strength: 80 ksi (552 MPa)
  • Wire Diameter: 5/32 in.
  • Amperage Range: 500 Amps - 900 Amps
  • Process: GMAW, SAW
  • Material: Mild Steel, Low Alloy
  • AWS Classification: AWS SFA 5.23: EF2
  • Trade Name: SPOOLARC 44