A question? Visit our contact page

Deoxidized Copper (ER Cu) MIG

  • Amperage Range: 150 - 250 A
  • Arc Voltage: 25 - 28 V
  • Wire Feed Speed: 200 - 320 ipm
  • Preheat Temperature: 1006F - 2006F
  • Gas Flow: 30 - 35 cfh
  • Diameter: 0.045 in
  • Weight: 10 lb
  • Spool Size: 8 in
  • Material: Deoxidized Copper
  • Alloy Type: ER Cu
  • Electrical Conductivity: 40% IACS
  • Tensile Strength: 29,000 psi
  • Hardness: 54 Brinell
  • Elongation: up to 30%
  • Melting Point: 19676F
  • Welding Process: GMAW (MIG)
  • Shielding Gas: Argon

Downloads

    Safety Data Sheet
    Spec Sheet