A question? Visit our contact page

Bare Silver (B Ag-7) BRAZING

  • Tensile Strength: 66,000 psi
  • Maximum Operating Temperature: 400°F continuous, 600°F intermittent
  • Solidus Temperature: 1145°F
  • Liquidus Temperature: 1200°F
  • Brazing Range: 1205 - 1400°F
  • Product Diameter: 1/16 in
  • Weight: 16 oz
  • Form: Coil
  • Alloy Type: Bare Silver (B Ag-7)
  • Silver Content: 55.0 - 57.0%
  • Copper Content: 21.0 - 23.0%
  • Zinc Content: 15.0 - 19.0%
  • Tin Content: 4.5 - 5.5%