Harris® 4043 Aluminum Silicon alloy is very commonly used to weld on 6XXX base materials and other heat treatable alloys. Harris® 4043 is a soft alloy, with good crack resistance and high penetration compared to other filler metals. It can be used for certain brazing applications and to weld on high silicon casts like A356. Welding of 5XXX base materials with 4043 and other 4XXX filler metals should be avoided.

Features

  • All-position welding
  • Designed for welding heat treatable base alloys, specifically 6XXX series alloys
  • Low sensitivity to weld cracking with the 6XXX series base alloys
  • Gray color (post anodized)
  • Often used for repair welding aluminum/silicon cast alloys such as grades 353/A356
  • Lower melting point and more fluidity than the 5XXX series filler alloys
  • Marked with model number on each end for easy identification after use
  • Common choice for welding 6061
  • Weight: 1.04 lbs
  • Tensile Strength: 27,000 psi (as welded 6061 base plate)
  • Yield Strength: 18,000 psi (as welded 6061 base plate)
  • Solidus Temperature: 1065 F (574 C)
  • Liquidus Temperature: 1170 F (632 C)
  • Material: Aluminum with 4.5-6.0% Silicon, max 0.30% Copper, max 0.20% Titanium, max 0.80% Iron
  • Welding Type: TIG (GTAW), MIG (GMAW)
  • Base Metal Compatibility: 6XXX series aluminum alloys, aluminum/silicon cast alloys (grades 353/A356)
  • Crack Sensitivity: Low crack sensitivity with 6XXX series alloys
  • Post Anodize Color: Gray
  • Density: 0.097 lbs/cu in

Downloads